| Item Number | Part Code | Nominal Element Size (mm) | Nominal Element Size (in) | Temperature Range °F | Temperature Range °C | Length (in) | Estimated ship* |
|---|---|---|---|---|---|---|---|
| U8770262 | WTD-5-1/2 | 13 | 0.5 | 350 | 175 | 0.5 | 5 weeks |
| U8770261 | WTD-5-1 | 13 | 0.5 | 350 | 175 | 1 | 6 weeks |
| U8770263 | WTD-5-1-1/2 | 13 | 0.5 | 350 | 175 | 1.5 | 14 days |
| U8770193 | HTD-5-1/2 | 13 | 0.5 | 500 | 260 | 0.5 | 5 days |
| U8770192 | HTD-5-1 | 13 | 0.5 | 500 | 260 | 1 | 5 weeks |
| U8770194 | HTD-5-1-1/2 | 13 | 0.5 | 500 | 260 | 1.5 | 5 weeks |
| U8770292 | VHTD-5-1/2 | 13 | 0.5 | 900 | 480 | 0.5 | 5 weeks |
| U8770291 | VHTD-5-1 | 13 | 0.5 | 900 | 480 | 1 | 5 weeks |
| U8770293 | VHTD-5-1-1/2 | 13 | 0.5 | 900 | 480 | 1.5 | 5 weeks |
| U8770259 | WTD-4-1/2 | 19 | 0.75 | 350 | 175 | 0.5 | 5 weeks |
| U8770258 | WTD-4-1 | 19 | 0.75 | 350 | 175 | 1 | 6 weeks |
| U8770260 | WTD-4-1-1/2 | 8 | 0.75 | 350 | 175 | 1.5 | 14 days |
| U8770190 | HTD-4-1/2 | 19 | 0.75 | 500 | 260 | 0.5 | 5 weeks |
| U8770189 | HTD-4-1 | 19 | 0.75 | 500 | 260 | 1 | 5 weeks |
| U8770191 | HTD-4-1-1/2 | 19 | 0.75 | 500 | 260 | 1.5 | 5 weeks |
| U8770289 | VHTD-4-1/2 | 19 | 0.75 | 900 | 480 | 0.5 | 14 days |
| U8770288 | VHTD-4-1 | 19 | 0.75 | 900 | 480 | 1 | 5 weeks |
| U8770290 | VHTD-4-1-1/2 | 8 | 0.75 | 900 | 480 | 1.5 | 5 weeks |
| U8770187 | HTD-3-1/2 | 25 | 1 | 500 | 260 | 0.5 | 5 weeks |
| U8770256 | WTD-3-1/2 | 25 | 1 | 350 | 175 | 0.5 | 5 weeks |
| U8770255 | WTD-3-1 | 25 | 1 | 350 | 175 | 1 | 5 weeks |
| U8770186 | HTD-3-1 | 25 | 1 | 500 | 260 | 1 | 5 weeks |
| U8770257 | WTD-3-1-1/2 | 25 | 1 | 350 | 175 | 1.5 | 14 days |
| U8770188 | HTD-3-1-1/2 | 25 | 1 | 500 | 260 | 1.5 | 5 weeks |
| U8770286 | VHTD-3-1/2 | 25 | 1 | 900 | 480 | 0.5 | 14 days |
| U8770285 | VHTD-3-1 | 25 | 1 | 900 | 480 | 1 | 5 weeks |
| U8770287 | VHTD-3-1-1/2 | 25 | 1 | 900 | 480 | 1.5 | 5 weeks |